New technology for characterization of multi-scale stress distribution in nickel-based single crystal superalloys

Views : 577
Author : Jazmyn
Update time : 2024-05-10 09:20:58

A nickel-based single-crystal superalloy is the preferred material for manufacturing high-pressure turbine blades, the core component of advanced aero engines. The residual stress generated during the preparation and processing of nickel-based single-crystal superalloys has a direct and important impact on the evolution of microstructure and degradation of mechanical properties during subsequent service. For example, some studies have found that in the early stages of thermal exposure or creep deformation, the rafting phenomenon of the γʹ coherent precipitation strengthening phase between dendrites and at the dendrite trunk shows significant asynchronous characteristics, which is likely to be related to the residual stress. The spatial distribution is uneven, and this residual stress includes both the coherent stress between the γ/γʹ phases and the stress at the dendrite scale. Therefore, in order to better understand the deformation mechanism of nickel-based single-crystal superalloys and optimize alloy design, it is necessary to measure the distribution of multi-scale stress with high precision and high spatial distribution.


 

However, as the most accurate stress measurement method recognized, X-ray diffraction technology has encountered huge challenges in the characterization of multi-scale stress distribution of nickel-based single crystal superalloys: the prerequisite for applying diffraction technology to measure stress is to know the stress-free state of the alloy material. The lattice constant d0 at Moreover, what is even more troublesome is that there are many types and high contents of alloying elements in nickel-based single crystal superalloys, especially elements such as W and Re which are unevenly distributed due to slow diffusion rates (segregation cannot be eliminated even after standard heat treatment), and thus This results in d0 being non-uniformly distributed, different everywhere and heavily dependent on the preparation conditions and thermal history of the alloy material, making it difficult to obtain. Even for the same alloy, changing the preparation method and heat treatment system may even change the sign of the two-phase lattice mismatch, which will lead to the inversion of tensile and compressive stresses and have a huge impact on mechanical properties.

In order to characterize the multi-scale stress distribution of nickel-based single-crystal superalloys, researchers from Xi'an Jiaotong University and the University of Science and Technology Beijing collaborated to develop a synchrotron radiation micro-beam diffraction method with sub-micron spatial resolution, which overcomes the inaccuracy of stress caused by unknown d0. Measurement problems, and taking nickel-based single crystal superalloy as an example, the characterization of the spatial distribution of microscopic stress in non-uniform coherent precipitation-strengthened alloys was achieved.
 
In this work, the author used the monochromatic light energy scanning technology of the synchrotron radiation microbeam line station to quantitatively characterize the lattice mismatch of the γ/γʹ phase in the nickel-based single crystal superalloy and calculated it based on this. Spatial distribution of coherent stress at the micron scale. In order to describe the effect of coherent stress on the sub-dendritic scale, the author based on the periodic structural characteristics of γʹ precipitate phase and γ phase channel in nickel-based single crystal superalloy, and used equivalent shrinkage to describe the effect of coherent stress on the precipitate phase scale. The resulting material deformation is then used to obtain the stress caused by the non-uniformly distributed coherent stress on the sub-dendritic scale using finite element simulation.

 

Figure 1. Characterization method of non-uniform microscopic stress. There is a dendritic structure (a) caused by element segregation in the nickel-based single crystal superalloy, in which the interdendritic (ID) part has no coherent stress (b) and the lattice distortion introduced (c), and the primary dendrite In the stem (PDA) and the secondary dendrite stem (SDA), the lattice mismatch at the coherent interface introduces coherent stress (d) and lattice distortion (e). Through the characterization of lattice distortion by synchrotron radiation microbeam diffraction energy scanning (f), coherent stress distribution with submicron spatial resolution can be obtained. Based on the equivalent shrinkage defined by coherent stress, finite element simulation can be used to obtain the stress (g) introduced by inhomogeneous coherent stress on the sub dendritic scale.

The study found that in the second-generation nickel-based single-crystal superalloy CMSX-4, even after standard heat treatment, the segregation of elements (especially the Re element) still caused a significantly uneven distribution of coherent stress. Such uneven distribution Coherent stress introduces uniaxial tensile stress along the dendrite growth direction in the secondary dendrite trunk. It forms a plane of compressive stress that balances the tensile stress in the inter-dendritic region.

 

Figure 2. Non-uniform distribution of mismatch degree and coherent stress in CMSX-4 nickel-based single crystal superalloy. (a) According to the segregation degree of Re, the primary dendrite trunk (PDA), secondary dendrite trunk (SDA) and interdendrite (ID) regions are divided. Lattice mismatch degree (b), coherent stress in the γ phase channel (c), and equivalent shrinkage caused by coherent stress (d) non-uniform distribution of dendrites.

By comparing the deviator strain tensor distribution measured by finite element simulation and synchrotron radiation microbeam Laue diffraction, the reliability of the simulation results is verified, and it is also proved that the sub-dendritic scale stress does originate from the non-uniformly distributed coherent stress.

 

Figure 3. Stress (a) and deviator strain distribution (b, c) along the [100], [010] and [001] directions. The gray dotted line divides the primary dendrite trunk (PDA) and the secondary dendrite trunk (SDA). ) and interdendritic (ID) regions. Comparing the finite element simulation (b) and the synchrotron radiation Laue microbeam diffraction measurement (c) deviator strain distribution can verify the correctness of the finite element simulation.

Through the method established in this study, the spatial distribution of coherent stress and sub-dendritic scale microscopic stress can be calculated simultaneously by characterizing the lattice mismatch degree when d0 is unknown; and this method is not only suitable for nickel-based high-temperature alloy and can also be extended to the research on other coherent precipitation strengthened alloys. Recent research has found that through composition design and process optimization, coherent precipitation-strengthened alloy materials with uneven alloy element distribution, precipitated phase morphology, and lattice mismatch can be prepared. This type of alloy is expected to have unparalleled mechanical properties. The multi-scale stress distribution characterization method established in this study is expected to provide strong support for the design and mechanical properties research of this type of alloy.

The relevant research results were published in Materials Research Letters under the title "Mapping stress heterogeneity in single-crystal superalloys by novel submicron-resolved X-ray diffraction." The first author of the paper is Kou Jiawei, a doctoral candidate in the School of Materials at Xi'an Jiaotong University. The corresponding authors are Professor Chen Kai of Xi'an Jiaotong University and Professor Wang Yandong of the University of Science and Technology Beijing. The co-authors include doctoral students Huang Shaoqi and Professor Zhai Chongpu of the School of Aerospace, Xi'an Jiaotong University, and Jiang Qingyou of Taiwan Light Source. Ph.D., associate researcher Wang Sisheng of Shanghai Light Source, researcher Li Zhijun of Institute of Applied Physics, Chinese Academy of Sciences.

 

Supplier

TRUNNANO is a globally recognized manufacturer and supplier of compounds with more than 12 years of expertise in the highest quality nanomaterials and other chemicals. The company develops a variety of powder materials and chemicals. Provide OEM service. If you need high quality 3D Printing Alloy Spherical Tungsten Nickel Iron Alloy Powder, please feel free to contact us. You can click on the product to contact us.
 
 

RNDKOREA | Sodium Silicate | Potassium Silicate | Spherical Alumina | Spherical SiO2 Powder | Zinc Sulfide ZnS Powder | 3D Printing Powder | Concrete foaming agent | Concrete Superplasticizer | Boron Nitride Powder | Nano Silicon Powder | CuO Powder | Cu2O Cuprous Oxide Powder | Cr2O3 Powder