Physical and chemical properties of cobalt phosphide Physical properties Cobalt phosphide is gray needle-like. Its relative density (15°C) is 6.14. The melting point is 1386°C. It is an efficient, stable and cheap transition metal phosphide. Chemical material Cobalt phosphide is soluble in nitric acid and aqua regia but insoluble in water. Cobalt phosphide (CO2P) is an intercalation compound formed by the phosphorus source entering the transition metal cobalt lattice. Cobalt phosphide can be used for magnetism, lithium battery anode material, hydrogenation catalysis and photocatalytic degradation, etc. Cobalt phosphide is a semiconductor material with a low bandgap, high thermal stability, chemical stability, strong electrical conductivity and high-efficiency catalytic performance, which meets the requirements of preparing high-efficiency water-splitting catalysts.Purity and particle size parameters of cobalt phosphide: Purity: 99.99% Particle size: -60 mesh Bulk density: 6.14 (g/cm3)
How is cobalt phosphide Co2P powder produced? Oil bath Trityl phosphorus is used as a phosphorus source to synthesize phosphate, which can be obtained in an organic mixture by thermal decomposition of metal phosphate. When tri octyl phosphorus is used as a phosphorus source in the reaction, it is easy to cause the agglomeration of the cobalt phosphate nanowires produced. Hydrogen reduction Since the bond between phosphorus and oxygen is stronger, phosphorus formation and oxygen metal and phosphorus bond only occur at high temperatures if the bond is broken, However, this process is easy to form metal particles, and the formation of metal particles greatly enhances the adsorption of hydrogen At the same time, the metal overflowed with phosphate, causing the phosphate to be reduced to phosphide. However, due to the high sintering temperature, the synthesis of phosphate via phosphate usually results in the formation of large grains mostly. Pyrolysis The relatively mild and simple hypophosphite pathway, that is, the decomposition of sodium hypophosphite by heating at high temperature (300-400°C), the toxic PH3 generated in situ will reduce the source of metal. Element preparation method Under hydrothermal conditions (140-200°C), phosphorus is used to prepare metal phosphides. Elemental phosphorus uses white phosphorus, yellow phosphorus and red phosphorus as phosphorus sources.
The price of cobalt phosphide TRUNNANO (aka. Luoyang Tongrun Nano Technology Co. Ltd.) is a trusted global chemical material supplier & manufacturer with over 12 years' experience in providing super high-quality chemicals and Nanomaterials. Currently, our company has successfully developed a series of powder materials. OEM service is available. If you are looking for Cobalt phosphidepowder, please contact us. Or click onthe needed products to send us an inquiry.